2
I am being considered for a position as a soil tech for a large grading project. I'm required to have knowledge of 'method spec'. Can anyone explain this to me? Your respnses are much appreciated.

I have spent a few years in a geotechnical lab running max-density curves and such, so I have a have a broad understanding of the industry, but limited field experience.
 
Replies continue below

Recommended for you

There are two types of specifications Performace Specifications and Method Specifications. Performances specs state that you will achieve a particular result, for example, lifts of 12 inches or less will achieve a compaction of 95% modified proctor. How that happens is up to the contractor. Method specs state the methods that will be used to construct the work. The fill will be placed in 6 inch lifts and rolled with 8 passes of a 10 ton roller. In this case the contractor is responsible to insure the proceedure is followed correctly, but is not held to a stanard of performance, such as a particular proctor value. Often project specs are a combination of both. I am not sure what they would want you to know, unless they want you to be able to document the construction to show conformance to a method specification.
"Construction of Fills" by Edward J Monahan published by Wiley is a good, short book that will give you some insight to the field side
Good luck.
 
That seems to clarify it for me, thank you kindly. I will at least be familiar with the term when I interview. And thanks for the book tip!
 
When you specify a method spec the contractor is not liable for failure to achieve specifications - whoever specified the method spec is.
 