What is polypropylene grade of sediment water filter ?

Status
Not open for further replies.
Replies continue below

Recommended for you

This PP grade material should be a grade to be injected (low Mw), it must be indicated to support the temperaturas indicated and should be certificated to be in contact with water.
 