I am a product engineer that makes drawings for parts that need to be vapor polished. In the past I have received parts that were spec’ed to be vapor polished, yet showed up not polished. The parts were buffed slightly so it was a bit hard to tell if they have been polished or not, this was the first time I had ordered the part, so it was hard to tell if it was polished or not. (Very small part, about the diameter of a BIC pen and a thickness of 0.053"). I used the parts thinking they were polished. Later to learn from the vendor they were not. This problem got sorted out, but in the future inspection will not be done by me, it will be done by a non-technical QA employee. How do I make sure they know what a polished part looks like? Give them a polished and a non-polished piece and allow them to do a visual comparison? My company is very small (I am 1 of 2 engineers) so we don't have a lot of cash for inspection equipment.
Thanks for any insight.