Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

when to follow ASTM A530 for hydrotest pressure calculations. 4

Status
Not open for further replies.

bck2ftr

Mechanical
Feb 7, 2014
13
In general for process piping ASME B31.3 is used for calculation of Hydrotest pressure.
Today I came across ASTM A530, which also specifies as
"each length of
pipe shall be tested by the manufacturer to a hydrostatic
pressure which will produce in the pipe wall a stress not less
that 60 % of the minimum specified yield strength for carbon
and ferritic alloy steel pipe, or 50 % of the specified minimum
yield strength for austenitic alloy steel pipe.
"

Can anyone clarify when to go for ASTM A530 method for a hydrotest?
 
Replies continue below

Recommended for you

ASTM A530 ( and just about any ASTM AXXX) is a pipe material standard. This includes a minimum test on the pipe after manufacture as part of the manufacturing process, commonly called "mill tests". It provides a very basic level of assurance that your pipe has been manufactured properly. You should therefore have few worries about the quality and integrity of your pipe.

B31.3 is a fabrication standard where various bits, including pipe, get joined together to form a system. This system is then hydrotested to prove its integrity after it has been fabricated. The code provides minimum requirements for the testing of this system which may or may not exceed the test level performed by the pipe vendor depending on the design pressure of the system.

The two should not be confused with each other.

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way
 
Good explanation LI.

David Simpson, PE
MuleShoe Engineering

In questions of science, the authority of a thousand is not worth the humble reasoning of a single individual. —Galileo Galilei, Italian Physicist
 
LittleInch, Thank you for the clarification
 
Thanks [thumbsup2]

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor