Hello, I have a new reboiler that will be going into service in a few months. The tube side is AL6XN and is in oil service (pH=5), the shell side is 316L and is in Dowtherm A service.
I have heard of pickling exchangers before, but do not know when it should be applied.
Are there some guidelines to determine when this is necessary?
Thank you,
I have heard of pickling exchangers before, but do not know when it should be applied.
Are there some guidelines to determine when this is necessary?
Thank you,