Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Toost on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

White Cast Iron Conversion Charts for Leeb Type "D" to HBW/HRC?

Status
Not open for further replies.

neuron1007

Materials
Feb 20, 2015
1
I've been trying to find data for approximate conversions between Leeb Hardness Numbers (Type D Device) and an indentation hardness method/scale (HBW, HRC, HV, etc), for high chromium white cast irons (e.g. BS4844 Grade 3D) specifically. Has anyone come across data comparing these HLD to one of the indentation scales for these alloys?
 
Replies continue below

Recommended for you

If it's not in ASTM E140 then I wouldn't know where to look. Ask a manufacturer maybe.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 
You can find many conversion tables on the internet, but none say that they are for high hardness case iron.
I would be very leery of using rebound hardness for a material that is as non-homogenous as a white iron.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Status