Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

who manufactures valves meeting Shell MESC standards?

Status
Not open for further replies.

sgrica

Industrial
Oct 11, 2005
2
I have been looking for a Bronze Valve that meets MESC Standards so far I have not found one and I have MESC Additional Requirement SPE 77/105 rev. 11-06-2001. I have tried Nibco, McDonald and Apollo. 2 q's 1. Is there a more up to date SPE 77/105? 2. Does SPE 77/105 also apply to Ball Valves ( doc says Globe, Check, Gate)? I would really appreciate any feed back.
 
Replies continue below

Recommended for you

SPE 77/105 is now dated 4th March 2005. It does not apply to ball valves; only to globe, gate, and check valves to BS 5154. In 1998, when Shell did have the sense to keep on top of its purchasing quality, the accepted suppliers were:
Bestobell
Crane Fluid
Hattersly Newman
Hender
Shipham

Steve Jones
Materials & Corrosion Engineer
 
Thanks SJones, that was a real help.
 