Is it possible to mold a thermoset to a thermoplastic with actual bonding occurring? This would be in a situation where mechanical interlocking was woefully neglected.
 
Replies continue below

Recommended for you

You could cure a thermoset like epoxy onto many types of thermoplastic and get good adhesion. You could melt a thermoplastic onto a thermoset but I would not expect good adhesion in that case due to lack of chemical bonding and proper wetting.

Chris DeArmitt PhD
President - Phantom Plastics LLC

Trusted adviser to leading companies around the world
 
Curing would be the way to go - I definitely need optimum adhesion. Thanks for your advice!
 