Does anyone have the A*E properties and weight for 7-19 wire rope or the area, weight and the E values for same? I'm looking for 1/2" dia to 1" dia for an Smath program

Thanks, Dik

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Replies continue below

Recommended for you

Thanks Gentlemen (Binary)... Contractor want to use wire rope for temporary guardrail...

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Thanks, Bridge...

PEinc... Wire rope, not prestressing cable... I think the contractor is opting for a 'tie-off' cable, not a 'cable guard'...

Joel... your reference has good information about the equivalent Young's modulus for different wire rope types...

again... thanks.

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 