Hi
In portable hardness test of a 28 inch WP11 tee we had some problem. As standards mentioned, before testing we should remove all oxides ,paint,.....
We prepare surface with a grinder till we visually see bright mirror like surface. The result of hardness test was 215 brinnel. We checked the thickness. By our first preparation ,the thickness decreased 0.1mm. I suggested to grind 0.1mm more and the results became within the range of standard ,about 170 brinnel.
Are we allowed to do the above mentioned process according to astm standards.
Thanks
In portable hardness test of a 28 inch WP11 tee we had some problem. As standards mentioned, before testing we should remove all oxides ,paint,.....
We prepare surface with a grinder till we visually see bright mirror like surface. The result of hardness test was 215 brinnel. We checked the thickness. By our first preparation ,the thickness decreased 0.1mm. I suggested to grind 0.1mm more and the results became within the range of standard ,about 170 brinnel.
Are we allowed to do the above mentioned process according to astm standards.