sb1999kb
Mechanical
- Feb 1, 2013
- 10
- 0
- 0
Hello all. I'm new to this forum and would like your help with a welding issue.
Question #1. If a welder has done performance qualifications for SMAW for the following:
P1 to P1 with F-3 & F-4, currently using 6010 root/7018 cover, would he also
qualify for 7010/8018 (all other variables are unchanged)?
Question #2. Does the code require a new WPS - PQR - WPQ?
Thanks for your kind assistance!
Question #1. If a welder has done performance qualifications for SMAW for the following:
P1 to P1 with F-3 & F-4, currently using 6010 root/7018 cover, would he also
qualify for 7010/8018 (all other variables are unchanged)?
Question #2. Does the code require a new WPS - PQR - WPQ?
Thanks for your kind assistance!