Is a WPS needed when placing weld-on CMU masonry anchors? If not is there a general standard anywhere for attaching these?
I see these things being welded on all the time and talk about your buggered up welds..these things meets none of the requirements of D1.1 Fig. 5.4 and arc strikes from top-to-bottom. These guys never met an arc strike that they wanted to incorporate into the weld.
I see these things being welded on all the time and talk about your buggered up welds..these things meets none of the requirements of D1.1 Fig. 5.4 and arc strikes from top-to-bottom. These guys never met an arc strike that they wanted to incorporate into the weld.