mulz
Mechanical
- Jul 15, 2015
- 18
Dear All,
I'm not expert in welding, Our submitted WPS/PQR got rejected by the client the reason is that the P-Number in WPS is not same with the PQR. WPS is P5A to P1 and the supporting PQR is P5A to P4.
From ASME SEC IX 2017: Qw-424.1 ''base metal used for Qualification: One metal from P-No. 5A to P no. 4 or P No. 3 or P No. 1 will qualify any P No. 5A to any metal assigned with P No. 4 or-3 or 1".
For what I have understand on that statement, our WPS is acceptable. Please correct me if I am wrong.
Thank in advance.
I'm not expert in welding, Our submitted WPS/PQR got rejected by the client the reason is that the P-Number in WPS is not same with the PQR. WPS is P5A to P1 and the supporting PQR is P5A to P4.
From ASME SEC IX 2017: Qw-424.1 ''base metal used for Qualification: One metal from P-No. 5A to P no. 4 or P No. 3 or P No. 1 will qualify any P No. 5A to any metal assigned with P No. 4 or-3 or 1".
For what I have understand on that statement, our WPS is acceptable. Please correct me if I am wrong.
Thank in advance.