soulglo
Marine/Ocean
- Feb 18, 2013
- 6
Hello all,
I need some information regarding a welding procedure for X52 pipe 25mm thick for a vessel's helideck legs
Our current procedure is for A333 material and uses ER80S-D2 tig wire and ER7018 electrodes.
I have 2 questions
Can this procedure be used for the X52 pipe as both are P-1 materials?
Can the ER80-D2 be substituted for ER70S-6 as both have the same F-No
Many thanks
I need some information regarding a welding procedure for X52 pipe 25mm thick for a vessel's helideck legs
Our current procedure is for A333 material and uses ER80S-D2 tig wire and ER7018 electrodes.
I have 2 questions
Can this procedure be used for the X52 pipe as both are P-1 materials?
Can the ER80-D2 be substituted for ER70S-6 as both have the same F-No
Many thanks