dman25
Materials
- Jun 17, 2008
- 5
We want to weld a X-65 cap to a X42/X52 duel grade pipe. I know according to API 1104 that when welding materials of two seperate material groups that the WPS for for the higher strength material is to be used.
My issue/question: Is procedure for X-65 allowable for the X42/X52 duel grade pipe. I'm thrown off by the X-42 since that would mean three different material groups. I have only dealt with going a group up or down but not jumping from group a to c.
Any guidance???
My issue/question: Is procedure for X-65 allowable for the X42/X52 duel grade pipe. I'm thrown off by the X-42 since that would mean three different material groups. I have only dealt with going a group up or down but not jumping from group a to c.
Any guidance???