Hi,
How I can use the function Young modulus vs temperature E=E(t)in the defining of the isotropic material (Nastran for Windows)?
With a lot of thanks,
Krzyszof
 
Replies continue below

Recommended for you

The modulus of elasticity of structural steel (E) is approximately 29,000 ksi at 70 deg F. It decreases linearly to about 25,000 ksi at 900 deg F and them begins to drop at an increasing rate at higher temperatures.

So it material dependent. Find numbers for material in question and make function.
 