Hi, would anyone have weld procedures for the ZeCor range of materials that could be applied to pipe sections, either using the SMAW or GTAW process or a combination of both?
Regards Pete
 
Replies continue below

Recommended for you

We have only ever used autogenous TIG on this alloy.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
thanks again; The conductor is aluminum (a good electrical conductor). (* Why neglects the component of z?)
So that at the end we have the component of x on account of the motion along the y-axis.
The conductor is thick (its dimensions 50 * 140 * 10 mm3).
And also the skin effect was neglected because of the movement at low speed.
thank you again
 
Hello Peter, I have a procedure for GTAW process. Send me an e-mail to: andres.tapiav@usach.cl