Just wondering if there are any other power plant folks out there who are ZLD. We are going through a lot of growing pains at my plant. Nalco has us switching from ferric sulfate as our primary coagulant in our clarifiers to a polymer coagulant that they sell. Has anyone else seen a similar situation?