Today at 3:46 PM #1 K KOram Mechanical Jan 22, 2025 2 Does anyone know the specs for this spline? on a drop arm. trying to repair one. Thank you ZF 1 5/8 x 36 ZGN 725 -Prep Bore is 35.50
Does anyone know the specs for this spline? on a drop arm. trying to repair one. Thank you ZF 1 5/8 x 36 ZGN 725 -Prep Bore is 35.50
Today at 6:20 PM #2 3DDave Aerospace May 23, 2013 10,853 Like these: https://petoletka.com/images/Drop Arms.pdf Are you planning to cut a tapered spline? From previous threads: https://www.eng-tips.com/threads/zgn-715.381292/ it is proprietary to a company named ZF. Upvote 0 Downvote
Like these: https://petoletka.com/images/Drop Arms.pdf Are you planning to cut a tapered spline? From previous threads: https://www.eng-tips.com/threads/zgn-715.381292/ it is proprietary to a company named ZF.
Today at 6:26 PM Thread starter #3 K KOram Mechanical Jan 22, 2025 2 Yes - I have to cut it - I think we can reverse engineer it using our CMM Upvote 0 Downvote
Today at 8:03 PM #4 3DDave Aerospace May 23, 2013 10,853 I would buy a new part, cut off the portion with the spline and then weld it to whatever it is you are making. Upvote 0 Downvote
I would buy a new part, cut off the portion with the spline and then weld it to whatever it is you are making.