Hello, everybody.
There is inside Nace MR0175/ISO15156(2):2009; A2.1.5 a mention about the metalic coatings. That is a not acceptable for preventing SSC. For standard we offer the bolts and nuts to attend NAce with Zinc plated. The material is correct with Nace (B7M-2HM). Our intention is not preventing SSC. Could we provide plated or nude bolts and nuts ?
There is inside Nace MR0175/ISO15156(2):2009; A2.1.5 a mention about the metalic coatings. That is a not acceptable for preventing SSC. For standard we offer the bolts and nuts to attend NAce with Zinc plated. The material is correct with Nace (B7M-2HM). Our intention is not preventing SSC. Could we provide plated or nude bolts and nuts ?