Thanks all,
Its the fabricator,who declares PAUT is not applicable as when we asked them to conduct PAUT in beginning, all joints got rejected and now instead of PAUT they are performing UT only in which We are not able to identify all the defects and joints are getting accepted. As per API 650...
Dear Experts,
Kindly let me know, Which NDT is feasible to proceed with accurate result of Flush Type Clean Out Doors of newly construction of water Tanks? We recommended contractor to conduct PAUT but they decline stating it will provide fake result as there is a gap of 1.5MM in the assembly of...