Dear Friends,
For AlMgSi0,7 F27 (6005) type alloy, I wonder about the quenching type of material at the press exit? Is water quenching necessary to catch up the mechanical strength value( it is about 270 MPa(tensile))
Thank you!!
Dear Expert Friends,
Some of our products, have pick up marks(defects) on them. We're observing pick-up effects during and after the extrusion process. I'm trying to solve this problem so I'm open for ideas and tips.
Thanks
Hello everbody,
During my researchs, DIN and EN standarts making lots of trouble to me about heat treatment processes, and wasting my time.
They're so confusing because of their differences. According to DIN standarts heat treatment at 6063 F22, 6063 F25 and in EN standarts 6063 T6, 6063 T66...