can anybody tell me the difference between the material 1.0619 and 1.7365.

Thank you in advance.
 
Replies continue below

Recommended for you

Hello,

WS 1.619 also known as GS-C25
Weight %
C=0.18-0.23
Si=0.60
Mn=0.50-1.20
P=0.03
S=0.02
equivalent to
ASTM A216 Gr. WCC

WS 1.7365 also known as GX15CrMo5
Weight %
C=0.25-0.30
Si=0.15-0.25
Mn=0.60-0.80
P+S=0.035 max
Cr=3.00-3.30
Mo=0.45-0.55




 