Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SDETERS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

1950s Lightweight Concrete Compressive Strength

Status
Not open for further replies.

sawoods

Structural
Aug 13, 2012
4
I am currently using original construction drawings from 1959 to determine whether or not a roof stucture can support new imposed loading. The drawings show a " 2" lightweight pre-cast concrete plank" roof deck. This is the only information the drawings contain concerning the roof deck. What strengths were they making back then that I could used for an assumed value of f'c for the concrete?
 
Replies continue below

Recommended for you

I've seen similar... max span approx 2'-6"... and f'c=3000 psi...

Dik
 
The supporting beams are at 6'-6" O.C. The concrete planks are only about 12" wide. One spot of spalling reveals some pretty heavy duty W.W.R., but otherwise, they seem to be in good shape. It seems like a pretty questionable system, but it's worked for over 50 years, with a ballasted roof until just recently, so it can't be all bad.

Thanks for the help.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor