Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

1950's slab contruction

Status
Not open for further replies.

mauri10

Structural
Oct 13, 2010
18
Has anyone worked with a 1950's slab system that calls for a 2" concrete on WWF lath and fireprofing?
 
Replies continue below

Recommended for you

V-rib form? Often used with 2 or 2-1/2" topping over owsj...

Dik
 
what does it mean "owsj"?, what is a V-rib form like?
Later renovations indicate a 2" conc slab and corrugated deck instead of a a 2" concrete on WWF lath and fireprofing as existing slab
 
open web steel joist = "owsj"

Regards,
Lutfi
 
On a 24" span, sounds like it might be formdeck with a concrete infill for the 2" depth.

Formdeck, at 1/2" to 1" deep, is not structural but for use as a permanent form only, and it is non-composite.