I'd like to specify a Cr-Mo reactor (8 ft diameter) which can potentially see 1150 F @ 50 psig. SO far various info I've found suggests we cannot go beyond 1050 F. Our internal pipe spec however says 2.25Cr-Mo is good up to 1200 F. Can gurus out there give me some advice?