We have a customer purchasing investment cast valve for recip pump valves in 8620, case hardened to 55-60Rc and wants to consider Chinese 20CrMnTi instead, to the same specs. Does anyone have experience with this material. How does it compare? Recommendations?
JSBC International, Inc.
 
Replies continue below

Recommended for you

Thanks OGMetEng,
I had read that thread, but thanks for responding.
I was looking for information, such as, comparison of harden ability, core hardness, cast ability, cost, corrosion resistance.
Thanks again,
Billy
 