Sir/s:
Our project has mistakenly using 316 Stainless Steel instead of 304 Stainless Steel (Drawing BOM 304 SS).
Our client recommend to cut all joints and change to 304 SS Pipes.
As we know that 316L has higher corrosion resistant than 304.
What can we suggest to our client in terms of Code? We are hoping that, if ever they just can consider not to cut the joints
and continue using the 316 SS welded to 304 (even if not as per drawing).
Thanks,
John
Our project has mistakenly using 316 Stainless Steel instead of 304 Stainless Steel (Drawing BOM 304 SS).
Our client recommend to cut all joints and change to 304 SS Pipes.
As we know that 316L has higher corrosion resistant than 304.
What can we suggest to our client in terms of Code? We are hoping that, if ever they just can consider not to cut the joints
and continue using the 316 SS welded to 304 (even if not as per drawing).