gguliye
Industrial
- Apr 17, 2019
- 115
Hi All,
is there any reasons why 316 SS spring is not possible to select for PSV in nace application while 316 SS nozzle or disc are possible to select?
regards,
is there any reasons why 316 SS spring is not possible to select for PSV in nace application while 316 SS nozzle or disc are possible to select?