Yasser emam
Mechanical
- Mar 24, 2019
- 1
This is the center main bearing journal of a CAT 3516 engine crankshaft and as you can see there are these colour stripes but by inspection with hand i can't feel any bitting or roughness.
This journal doesn't have oil hole
Anybody have seen this before?
What is the cause of it?
Is it normal, abnormal or critical condition?
This journal doesn't have oil hole
Anybody have seen this before?
What is the cause of it?
Is it normal, abnormal or critical condition?