Greetings!
We need urgent help
6 pcs of 38" triple-offset butterfly valves are passing (more than 50% of number installed). The valves worked fine for about 12 months. Increasing the torque from 75% to 100% didn't help.
Service: isolation valves for mercury removal filters (dry natural gas)
Class 600#
Pop = 66 barg
DP = 76 barg
Top = 25 C
DT = 82 C
Materials:
body = A351 CF8M
seat = 316SS / Graphite
Plant is 1 year old, there is a possibility of large quantity of dust / scale in the piping. In theory, these valves should be somewhat OK with solids in process fluid.
I haven't had a chance to talk to the OEM, will do that tomorrow.
Any comments on cause, rectification would be much appreciated. If you need more info please advise.
Thank you,
S.
We need urgent help

6 pcs of 38" triple-offset butterfly valves are passing (more than 50% of number installed). The valves worked fine for about 12 months. Increasing the torque from 75% to 100% didn't help.
Service: isolation valves for mercury removal filters (dry natural gas)
Class 600#
Pop = 66 barg
DP = 76 barg
Top = 25 C
DT = 82 C
Materials:
body = A351 CF8M
seat = 316SS / Graphite
Plant is 1 year old, there is a possibility of large quantity of dust / scale in the piping. In theory, these valves should be somewhat OK with solids in process fluid.
I haven't had a chance to talk to the OEM, will do that tomorrow.
Any comments on cause, rectification would be much appreciated. If you need more info please advise.
Thank you,
S.