Currently, i am checking the viability of 4 lane of RCC T beam bridge. The features of bridge are:
Span= 25m
No. of longitudinal girder =6
Depth of longitudinal girder = 2.5m
I have modeled in sap and done manual calculation.
The live load distribution among the longitudinal girder was done by Little and morrice method as well as K.S. rakshit method to check the authenticity of the manual calculation.
The distribution coefficient for outer most longitudinal girder (spacing 3.28m) was found to be 1.64 by little and morrice method.
The distribution coefficient for outer most longitudinal girder (spacing 3.28m) was found to be 1.6 by K.S. Rakshit method.
The bending moment due to 2 number of 70R (W) assuming a single beam elemnet was found to be 9256.4 KN-m.
Here the softwatre and manual calculation result matches.
However, upon checking the software for outer longitudinal girder, the bending moment value is 4208 KN-m
BUt manual calculation shows, the value of bending moment of 2783 KN-m.
Currently, i am checking the viability of 4 lane of RCC T beam bridge. The features of bridge are:
Span= 25m
No. of longitudinal girder =6
Depth of longitudinal girder = 2.5m
I have modeled in sap and done manual calculation.
The live load distribution among the longitudinal girder was done by Little and morrice method as well as K.S. rakshit method to check the authenticity of the manual calculation.
The distribution coefficient for outer most longitudinal girder (spacing 3.28m) was found to be 1.64 by little and morrice method.
The distribution coefficient for outer most longitudinal girder (spacing 3.28m) was found to be 1.6 by K.S. Rakshit method.
The bending moment due to 2 number of 70R (W) assuming a single beam elemnet was found to be 9256.4 KN-m.
Here the softwatre and manual calculation result matches.
However, upon checking the software for outer longitudinal girder, the bending moment value is 4208 KN-m
BUt manual calculation shows, the value of bending moment of 2783 KN-m.