Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

7075-T79511 Extrusion

Status
Not open for further replies.

PASiii

New member
Apr 26, 2004
1
Does anyone know where I can find mechanical properties for 7075-T79511 extruded aluminum? Any help is greatly appreciated.
 
Replies continue below

Recommended for you

Since this is not a common product, I would contact Alcoa.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
PASiii

I would like to know if you were successful in your attempt to obtain the 7075-T79511 extrusion allowables data? This material is used in the wet areas of the Airbus narrow body aircraft and I too would really like to get my hands on it.

FYI it is my understanding that the static strength properties are very similar to 7075-T6511 extrusion, with better corrosion resistance.
 