HI,
I am trying to get two AM simulations working in Abaqus 2021. One is with a concentrated moving heat source, and the other is with a Goldak heat source model. The concentrated source works fine, but when I run the Goldak model, it throws a memory error after 10 increments. My device has enough memory, I have not changed any other parameters except for the moving heat source values and my model is also quite small to create any memory errors. Help me find what the issue is, please.
I am trying to get two AM simulations working in Abaqus 2021. One is with a concentrated moving heat source, and the other is with a Goldak heat source model. The concentrated source works fine, but when I run the Goldak model, it throws a memory error after 10 increments. My device has enough memory, I have not changed any other parameters except for the moving heat source values and my model is also quite small to create any memory errors. Help me find what the issue is, please.