Has anyone ever had problems with installing ABS pipework in a chilled water application. We have recently installed varying pipe sizes on a complete installation ranging from 32mm dia to 200mm dia. We have had 5 joint failures (in the 50mm dia pipework only)and one failure which appeared to the naked eye to be a failure on a crack down the longitudinal section of the pipe. Analysis by the manufacturers chemist has stated the failures are due to the prescence of a very small quantity of an unspecified alkyl ester which i understand to be a man made mineral oil. Durapipe's (the manufacturer) technical data makes no reference to this being a potential problem. Can anyone tell me of similar experiences