For Type B Air Meter, how much leakage is acceptable?
I know that as the cir cools, it will lose a little pressure, but after allowing some time for the air to cool, how much leakage is acceptable? If the gauge needle drop 0.1 % in a say 30 seconds, is that OK? Most air meters I see have a little leakage, but 20-30 seconds seems like a reasonable time to run the test.Did i miss something in the Standard?
I know that as the cir cools, it will lose a little pressure, but after allowing some time for the air to cool, how much leakage is acceptable? If the gauge needle drop 0.1 % in a say 30 seconds, is that OK? Most air meters I see have a little leakage, but 20-30 seconds seems like a reasonable time to run the test.Did i miss something in the Standard?