Hi!,

Could someone tell me what is the most similar to Alloy 20 or S32615 (SX) available in alloy material's ´pipe listed in Caesar ii?

Best regards.
 
Replies continue below

Recommended for you

Alloy 20 is SB-729 N08020, Caesar material 394. S32615 is an unlisted material so that's a bit trickier but you may need to add it to your material library.
 