KootK
Structural
- Oct 16, 2001
- 18,674
Disclaimer: I am using this post as a means to expedite / circumvent my own research. I do realize that Google is my friend. I'm a little pressed for time and resources unfortunately.
So... I've got some 4 m tall aluminum public art that needs to be connected to a concrete grade beam. And I'm not an aluminum expert by any means. I'd appreciate any advice here regarding the design of this connection. Things that I'm concerned about:
1) Fatigue in the pole / base plate connection.
2) Vibration issues similar to those encountered with light standards.
3) Aluminum / concrete corrosion. What needs isolating from what here and how would that best be accomplished?
4) For something of this scale, I don't need to debond/prestress the anchor bolts for fatigue resistance do I?
5) Anything that I should know about RHS section availability?
6) Anything I should know about aluminum welding?
7) Any issues with tight radius bending of aluminum pipe (wall thickness)?
That's a long list, I know. Feel free to answer any item that tickles your fancy without addressing the rest. And, if you can think of anything that should be added to my list, don't hesitate to table it.
I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
So... I've got some 4 m tall aluminum public art that needs to be connected to a concrete grade beam. And I'm not an aluminum expert by any means. I'd appreciate any advice here regarding the design of this connection. Things that I'm concerned about:
1) Fatigue in the pole / base plate connection.
2) Vibration issues similar to those encountered with light standards.
3) Aluminum / concrete corrosion. What needs isolating from what here and how would that best be accomplished?
4) For something of this scale, I don't need to debond/prestress the anchor bolts for fatigue resistance do I?
5) Anything that I should know about RHS section availability?
6) Anything I should know about aluminum welding?
7) Any issues with tight radius bending of aluminum pipe (wall thickness)?
That's a long list, I know. Feel free to answer any item that tickles your fancy without addressing the rest. And, if you can think of anything that should be added to my list, don't hesitate to table it.
I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.