gmarken
Mechanical
- Oct 13, 2004
- 83
Does anyone know if AMS-4777 Nickel Alloy is compatible with a 35% peroxide solution? I have been searching but cannot find a definitive answer.
I plan on using this material in a furnace brazed assembly of several pieces of 316 stainless steel. 316 is good with peroxide so I need to verify the filler material is acceptable.