Hi All,

Have anyone heard the terms before, APCS? I believe it means "Approved Protective Coating System"

Check google but it did not have any related information, same goes to the website like IHS.

Anyone have information on this coating term?

Thanks,
Jeffrey
 
Replies continue below

Recommended for you

Saudi Aramco Engineering Standard SAES-H-101 - Approved Protective Coating Systems For Industrial Plant & Equipment. At least it was called that in 2005.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Yes it is Saudi Aramco approved coating systems. That ranges from APCS 1, 1A, 1B , 2A .. upto 26T
Different kind of applications, different paint systems. Still the most reliable paint specs in GCC



For Reference Just go through the attached
 
 http://files.engineering.com/getfile.aspx?folder=1825b4aa-1238-447d-88b0-4977d003d397&file=HEMPEL_PRICE_SHEET.xlsx
Thanks Gregorydas! Truely appreciated. =)
 