Dear all,

I am looking for material for flange which suitable for API 5L X46 pipe class.
My customer ask casted material and they sent me this:

ASTM A494 F46

I have not found any F46 in this material spec.

Can you recomended something?

Thank you

 
I think this is a typo. Try A 694.

My motto: Learn something new every day

Also: There's usually a good reason why everyone does it that way
 
Thank you very much.
I spent hours on it.

Regrads

elmio
 
Hi.

The material must be A694 F46.

greetings to all.

 
Thank you hfpolo!

It was a typing error by customer. Our sales team did enough mistake that case I did not want ask back to the customer.

Regards

Elmio
 