They have the same mechanical properties which is the criterion to select
Conditions
Pipe oleoducte oil: service: diesel, gas90, naphta
Pressure 1000 psi
Temperature : 50 celsius
Length : 7 km
Pipe oleoducte oil: r7. heavy oil
Pressure 1000 psi
Temperature : 50 celsius
Length : 7 km
Best regards for all your comments
Conditions
Pipe oleoducte oil: service: diesel, gas90, naphta
Pressure 1000 psi
Temperature : 50 celsius
Length : 7 km
Pipe oleoducte oil: r7. heavy oil
Pressure 1000 psi
Temperature : 50 celsius
Length : 7 km
Best regards for all your comments