Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API579/ASM FFS Table F.12 - Fatigue Crack Growth Data for Use With the Bilinear Equation 1

Status
Not open for further replies.

jkampman

Mechanical
Jun 23, 2022
2
Figure F.8 shows the growth rate curve at Regime C to be steeper than at Regime B.
However, the parameters in Table F.12(M) result in a less steep curve for the Upper stage compared to the lower stage.
Does anyone understand this?
 
Replies continue below

Recommended for you

Hi jkampman,
The lower and upper stage crack growth curves for a bilinear fatigue crack growth model both still relate to the 'Regime B' striation growth behavior. In that Figure it shows a linear growth for simplicity.
P.S, it seems that you are using an older version of API 579-1/ASME FFS-1 (2007?), I would recommend using the latest version which is API 579-1/ASME FFS-1 2021.
 
Hi danb3,
Thanks for the clarification (and the version tip)! Do you know if there is a way to determine where regime B ends and regime C starts?
 
Status