Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Appying a finish to aluminium

Status
Not open for further replies.

eski1

Mechanical
Jun 15, 2004
90
Hi

I am making some bespoke aluminium cabinets that are going to be made from 10mm aluminium 6082 tooling plate & sent to a polishers to apply a brushed finish.
I have attached a picture to show you the sort of thing we are making.

The Brushing process would leave the aluminium exposed & because these cabinets are going in a shop and will be handled the client is worrying about what will happen to them over time .
So they have asked what we can do about this , the brushing leaves a Matt finish which they want to retain so I guess this negates us using a clear lacquer.
I was hoping we could just apply a wax or spray that can be applied at the assemble stage in the shop but this might be wishful thinking .

So my questions are :-
Would the aluminium oxidize & mark easily over time in a dry retail shop ?
If so what could we do to stop this ?

any help would be greatly appreciated.
 
 http://files.engineering.com/getfile.aspx?folder=9f918cfa-e796-4ecf-a53f-17e6679448cc&file=box_joint.JPG
Replies continue below

Recommended for you

It is possible that the aluminium surfaces will get marked and corroded over time. It will depend upon what comes in contact with the surfaces. One option to consider is clear anodizing, which should retain some of the original brushed roughness and appearance.
 