bridgeDisciple
Electrical
- Jun 2, 2022
- 20
I'm hoping for some shared wisdom here. I'm designing a bridging system for an autonomous transit network (ATN) - light-weight modern form of APM. It is roughly in the class of pedestrian bridge with light vehicle capability, and similar in form to pony truss bridges with outboard walkways. The section is a box truss. "Cross ties" attached atop the pony cross truss extend horizontally "outboard" beyond the box, upon which the tracks are mounted. So torsional loading of the box section mid-span is a concern.
Steels, welds, and calculations for bridges are more extreme than for other structures because 1- they are exposed to weather, and 2- they are subject to extreme fatigue loads. But AASHTO and AISC guidance is a little weak on advisability of using HSS chords. The bridging is also extremely cost sensitive, so manufacturability is a key consideration.
I like the idea of HSS for aesthetics, torsion resistance, and buckling resistance. But those inner surfaces pose a long term potential hidden corrosion challenge. The ability to seal off the HSS ends to corrosion protect them seems in doubt, yet the standard docs suggest use is widespread enough that "guidance is coming".
So if any of you old bridge hands would like to steer me in the right direction, i'd appreciate it. Should i stick to angles, WT, or small beams ? Or is an HSS chorded box truss a reasonable choice ?
Steels, welds, and calculations for bridges are more extreme than for other structures because 1- they are exposed to weather, and 2- they are subject to extreme fatigue loads. But AASHTO and AISC guidance is a little weak on advisability of using HSS chords. The bridging is also extremely cost sensitive, so manufacturability is a key consideration.
I like the idea of HSS for aesthetics, torsion resistance, and buckling resistance. But those inner surfaces pose a long term potential hidden corrosion challenge. The ability to seal off the HSS ends to corrosion protect them seems in doubt, yet the standard docs suggest use is widespread enough that "guidance is coming".
So if any of you old bridge hands would like to steer me in the right direction, i'd appreciate it. Should i stick to angles, WT, or small beams ? Or is an HSS chorded box truss a reasonable choice ?