Hi all,
I have a problem I would like to have better understanding of. Its a flat slab design supported on columns. I am using Protastructure to analyse the slab by FE method. The result is showing the contour of the top hogging reinforcement near the column.
Here is a snapshot of the top reinforcement.
How should I tackle this in terms of providing reinforcement to the slab? There is a high concentration of steel required at two corners while the rest of the area only require minimal reinforcement. Would you apply the maximum steel required based on this design for the column strip? Thanks in advance.
Al
I have a problem I would like to have better understanding of. Its a flat slab design supported on columns. I am using Protastructure to analyse the slab by FE method. The result is showing the contour of the top hogging reinforcement near the column.
Here is a snapshot of the top reinforcement.

How should I tackle this in terms of providing reinforcement to the slab? There is a high concentration of steel required at two corners while the rest of the area only require minimal reinforcement. Would you apply the maximum steel required based on this design for the column strip? Thanks in advance.