Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME B31.3 Table 323.3.1 WPS thickness range

Status
Not open for further replies.

kripton

Materials
Aug 9, 2016
12
Hello,
Question is determination of wps thickness range.
pipe type/size : A333GR6 6'' sch 60 (9.53mm)
impact test req. :yes -40.
Process: Gtaw/Smaw

So what is the wps min/max thickness range qualified shall be?
according ASME B31.1 Table 323.3.1 to t/2 to t+6mm ?
4.765mm - 15.53mm
or
according to Section IX QW 403.6 ?
9.53mm - 19.06mm

Thank you for the help.
 
Replies continue below

Recommended for you

You reference table 323.3.1, but mention B31.1. Can we assume youre using B31.3?

/edt. Table 323.3.1 is for the size of the specimen to be impact tested: one piece (thickness T) for each range of thickness T/2 to T + 6 mm.
 
Thank you for the reply?
In which cases QW-403.6 applies?
 
If the project is built in accordance with B31.3, then the T/2 to T + 6mm rule applies.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor