ipi
Petroleum
- Nov 24, 2004
- 25
I recently saw a WQT qualified with unassigned to p43 and extend their range of qualification as unassigned to P1 to 15f, 34, 41 to 49.,
As per the table given in QW-423.1 , I understand than any unassigned to any p number qualifies for same p number only, and in this case limited to p43 only.
Your valuable insight regarding the range qualified is welcome
Thanks
As per the table given in QW-423.1 , I understand than any unassigned to any p number qualifies for same p number only, and in this case limited to p43 only.
Your valuable insight regarding the range qualified is welcome
Thanks