I recently saw a WQT qualified with unassigned to p43 and extend their range of qualification as unassigned to P1 to 15f, 34, 41 to 49.,

As per the table given in QW-423.1 , I understand than any unassigned to any p number qualifies for same p number only, and in this case limited to p43 only.

Your valuable insight regarding the range qualified is welcome

Thanks


 
Replies continue below

Recommended for you

Your understanding is correct - the WQT is incorrect.
 
Thanks Dekdee.