Jan 7, 2024 #1 nabeel3 Mechanical Dec 14, 2006 122 0 16 SA Dear Experts, In ASME Sec IX QW 451.1 is for the Transverse bend test and 451.2 longitudinal bend test. How can we decide when I have a specimen of thickness "t" which bend test is to be performed?
Dear Experts, In ASME Sec IX QW 451.1 is for the Transverse bend test and 451.2 longitudinal bend test. How can we decide when I have a specimen of thickness "t" which bend test is to be performed?
Jan 8, 2024 #2 r6155 Mechanical Jan 12, 2010 2,677 0 36 AR See QW-161.1 and .2 Regards Upvote 0 Downvote